Polymer Property : Fatigue Strength = 300 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 300 MPa

@# of Cycles 1.00e+7
43500 psi

@# of Cycles 1.00e+7
RB R=-1
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Forged Plate
Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part..