Polymer Property : Fatigue Strength = 296 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 296 MPa

@# of Cycles 1.00e+6
43000 psi

@# of Cycles 1.00e+6
American Utility Metals Cromgard® Stainless Steel
Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o..
Fatigue Strength 296 MPa

@# of Cycles 4.00e+6
43000 psi

@# of Cycles 4.00e+6
American Utility Metals Cromgard® Stainless Steel
Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o..
Fatigue Strength 296 MPa

@# of Cycles 1.00e+7 ,
Temperature 454 °C
42900 psi

@# of Cycles 1.00e+7 ,
Temperature 849 °F
AK Steel 410 Martensitic Stainless steel
AK Steel 410 provides good corrosion resistance plus high strength and hardness. It is magnetic in both annealed and hardened conditions. A wide range of properties can be developed with different..