Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 282 MPa @# of Cycles 1.00e+7 |
40900 psi @# of Cycles 1.00e+7 |
notched |
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 20% Elongated Alpha + STA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 20% Elongated Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL.. |
|||
Fatigue Strength | 282 MPa @# of Cycles 1.00e+7 |
40900 psi @# of Cycles 1.00e+7 |
notched |
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + Annealed This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + Annealed (705°C/1hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4-6. .. |