Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 276 MPa @# of Cycles 1.00e+7 |
40000 psi @# of Cycles 1.00e+7 |
notched |
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Elongated Alpha + STA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Elongated Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL.. |
|||
Fatigue Strength | 276 MPa @# of Cycles 1.00e+7 |
40000 psi @# of Cycles 1.00e+7 |
notched |
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL®.. |
|||
Fatigue Strength | 276 MPa @# of Cycles 3000 |
40000 psi @# of Cycles 3000 |
Flexural Fatigue (SN) |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |