Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | <= 237 MPa @# of Cycles 1.00e+7 |
<= 34400 psi @# of Cycles 1.00e+7 |
|
ArcelorMittal 06 High formability steel for drawing, Cold rolled Available in the following: uncoated (DC06) and electroglavanized (DC06+ZE) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These product.. |