Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 220.9 MPa @Temperature 20.0 °C |
32040 psi @Temperature 68.0 °F |
P50% rotary bending values for 5X10<sup>7</sup> cycles |
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T6 Heat Treatment Condition T6 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |