Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 207 MPa @# of Cycles 1.00e+7 |
30000 psi @# of Cycles 1.00e+7 |
Smooth |
Alcoa 2090-T83 Aluminum Aluminum-lithium alloy developed for high strength aerospace applications. The Al-Cu-Li alloy offers an 8 per cent density savings when compared with other aerospace alloys. Alloy 2090-T83 also has .. |
|||
Fatigue Strength | 207 MPa @# of Cycles 1.00e+7 |
30000 psi @# of Cycles 1.00e+7 |
Longitudinal, R.R. Moore rotating beam, fully reversed cycles with R = 0.1 |
Materion AlBeMet® AM 162 Extruded Bar, Annealed Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube.. |