Polymer Property : Fatigue Strength = 186 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 186 MPa

@# of Cycles 1.00e+7 ,
Temperature 538 °C
27000 psi

@# of Cycles 1.00e+7 ,
Temperature 1000 °F
AK Steel 410 Martensitic Stainless steel
AK Steel 410 provides good corrosion resistance plus high strength and hardness. It is magnetic in both annealed and hardened conditions. A wide range of properties can be developed with different..