Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 115 MPa

@# of Cycles 100 ,
Temperature 140 °C
16700 psi

@# of Cycles 100 ,
Temperature 284 °F
R = 0.1, 8 Hz, dry
DSM Stanyl® TW200B6 PA46-CF30
30% Carbon Reinforced, Heat Stabilized, Lubricated