Mechanical Properties Metric English Comments
Fatigue Strength <= 1030 MPa

@# of Cycles >=1.00e+7
<= 150000 psi

@# of Cycles >=1.00e+7
QuesTek® Innovations Ferrium® C61™ Case-hardened Gear Steel with Ultrahigh-strength Core
Description: Ferrium® C61™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the ..