Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 145 MPa @# of Cycles 1.00e+6 |
21000 psi @# of Cycles 1.00e+6 |
T-L |
Aleris AA5024-H116 Aluminum Magnesium Scandium Alloy Features good weldability, excellent damage tolerance, good corrosion resistance, creep-formability. Aleris AlMgSc alloy AA5024 H116 allows simplification of the manufacturing process of aircraft f.. |
|||
Fatigue Strength | 145 MPa @# of Cycles 300000 |
21000 psi @# of Cycles 300000 |
T-L |
Aleris AA5024-H116 Aluminum Magnesium Scandium Alloy Features good weldability, excellent damage tolerance, good corrosion resistance, creep-formability. Aleris AlMgSc alloy AA5024 H116 allows simplification of the manufacturing process of aircraft f.. |
|||
Fatigue Strength | 145 MPa @# of Cycles 100000 |
21000 psi @# of Cycles 100000 |
Notched (K<sub>T</sub> = 3) |
Alcoa 2090-T83 Aluminum Aluminum-lithium alloy developed for high strength aerospace applications. The Al-Cu-Li alloy offers an 8 per cent density savings when compared with other aerospace alloys. Alloy 2090-T83 also has .. |