Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 98.4 MPa @Temperature 150 °C |
14300 psi @Temperature 302 °F |
P50% rotary bending values for 5X10<sup>7</sup> cycles |
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T6 Heat Treatment Condition T6 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |