Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | <= 931 MPa @# of Cycles >=1.00e+7 |
<= 135000 psi @# of Cycles >=1.00e+7 |
|
QuesTek® Innovations Ferrium® C61™ Case-hardened Gear Steel with Ultrahigh-strength Core Description: Ferrium® C61™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the .. |
|||
Fatigue Strength | <= 930 MPa @# of Cycles 100000 |
<= 135000 psi @# of Cycles 100000 |
|
ArcelorMittal MartINsite® 1500 Cold Rolled Steel Description: The family of MartINsite steels extends ArcelorMittal's range of Ultra High Strength Steels (UHSS). These steels allow the realization of lightweight structural elements by a forming me.. |