Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 79.8 MPa @# of Cycles 10719 , Temperature 100 °C |
11600 psi @# of Cycles 10719 , Temperature 212 °F |
DAM; 5Hz,R=0.1; 4mm; ISO 13003 |
DuPont Performance Polymers Zytel® HTN FE350038 BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFE350038 BK083 is a 33% glass reinforced, heat stabilized, lubricated, hydrolysis resistant high performance polyamide resin, developed for improved structural performance. It is also a P.. |
|||
Fatigue Strength | 80.0 MPa @# of Cycles 1.00e+8 |
11600 psi @# of Cycles 1.00e+8 |
test bar (22mm diam.) notched (Kt = 3) |
Superior Die Set FORTAL® HR Aluminum Alloy Description: FORTAL is a high strength, lightweight, easy to machine alloy, originally developed to be used in the aerospace industry. It can be found whenever a structure is highly solicited and d.. |