Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 63.8 GPa | 9250 ksi | |
California Fine Wire Alloy 20-245 Precious Metal Alloy All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireInsulatedInformation provided by California Fine Wire. |