Mechanical Properties Metric English Comments
Modulus of Elasticity 3.00 - 9.80 GPa

@Temperature 60.0 - 150 °C
435 - 1420 ksi

@Temperature 140 - 302 °F
Average value: 5.86 GPa Grade Count:2
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..