Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.565 GPa | 82.0 ksi | |
Abatron ROCKWELD 55-27 A/B Structural Adhesive Putty; Epoxy ROCKWELD 55-27 is a 2-component epoxy system with low density, high-strength, and no shrinkage. It is a structural adhesive putty for sculpturing, repairs and restoration of stone, concrete and maso.. |