Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 8.40 - 11.6 GPa | 1220 - 1680 ksi | Average value: 9.93 GPa Grade Count:15 |
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum .. |
|||
Modulus of Elasticity | 8.40 GPa | 1220 ksi | ISO 527-1/-2 |
BASF Ultramid® S3EG6 Balance 30% Glass Filled PA 610 (Dry) Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. .. |
|||
Modulus of Elasticity | 8.40 GPa | 1220 ksi | ISO 527-1/-2 |
BASF Ultramid® S3WG6 Balance 30% Glass Filled PA 610 (Dry) Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. .. |