Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 79.0 GPa | 11500 ksi | |
Schott N-KZFS11 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 79.0 GPa | 11500 ksi | |
Schott N-SK11 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 79.0 GPa | 11500 ksi | |
Alcoa Deltalloy® 4032-T651 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = B; General Corrosion Resistance = C (A = best; E = worst). General 4032 characteristics and uses: Good machinability and drilling characterist.. |
|||
Modulus of Elasticity | 79.0 GPa | 11500 ksi | |
Alcoa Deltalloy® 4032-T86 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = B; General Corrosion Resistance = C (A = best; E = worst). General 4032 characteristics and uses: Good machinability and drilling characterist.. |