Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 76.5 GPa @Temperature 649 °C |
11100 ksi @Temperature 1200 °F |
|
Latrobe Lescalloy® D6AC VAC-ARC High Strength Alloy Steel LESCALLOY D6AC VAC-ARC steel is a medium carbon, low alloy, ultra high strength steel primarily designed for high strength structural applications requiring strength leaves up to 280,000 psi. This .. |