Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 51.0 GPa | 7400 ksi | |
Schott Glass 8337B Borosilicate Glass Borosilicate glass for sealing to Kovar metal and tungsten, highly UV-transmitting photomultiplier and UV detectors The heavy metal content for the elements lead, cadmium, mercury, and hexavalent .. |
|||
Modulus of Elasticity | 51.0 GPa | 7400 ksi | |
Corning 7070 Lithia Potash Borosilicate Crushed/Powdered Glass Available in mesh sizes 4 through 325 and can be customized. Devitrifies before reaching a softening point. Used for sealing and other applications.Information provided by Corning Incorporated. |