Polymer Property : Modulus of Elasticity = 74.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 74.0 GPa
10700 ksi
Schott N-PK51 Glass
Suitable for precision moldingInformation Provided by SCHOTT North America, Inc.
Modulus of Elasticity 74.0 GPa
10700 ksi
Saint-Gobain HS Grade Optical Fused Quartz
HS Grade Optical Fused Quartz is a high purity, low [OH] natural fused quartz. It has excellent IR transmission, useful transmission from 260 to 3500 nm, excellent visual quality with low bubbles, ..
Modulus of Elasticity 74.0 GPa
10700 ksi
Saint-Gobain Spectrosil® 1000 Optical Fused Quartz
Spectrosil® 1000 grade is used for non-transmissive mirrors and substrates, and other high purity components which do not require specified optical transmission.Spectrosil® is a synthetic fuse..
Modulus of Elasticity 74.0 GPa
10700 ksi
Saint-Gobain Spectrosil® 2000 Optical Fused Quartz
Spectrosil® 2000 is a deep UV, fluorescence-free grade.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually chlor..
Modulus of Elasticity 74.0 GPa
10700 ksi
Saint-Gobain Spectrosil® 2100 Optical Fused Quartz
Spectrosil® 2100 has improved refractive index homogeneity.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually c..
Modulus of Elasticity 74.0 GPa
10700 ksi
Saint-Gobain Spectrosil® 2200 Optical Fused Quartz
Spectrosil® 2200 grade is an excimer laser grade developed for maximum transmission and prolonged life in microlithography and other critical deep UV applications using KrF (248 nm) and ArF (193 ..
Modulus of Elasticity 74.0 GPa
10700 ksi
Saint-Gobain Vitreosil® 055 Optical Fused Quartz
Vitreosil® 055 is the highest grade of optical grade fused quartz available from Saint-Gobain Quartz for use in the near UV and visible. It has a useful transmission range from 270 nm in the nea..
Modulus of Elasticity 74.0 GPa
10700 ksi
Saint-Gobain Vitreosil® 065 066 Optical Fused Quartz
Vitreosil® 065, for use in the near UV and visible, has a less rigorous bubble specification. It has a useful transmission range from 270 nm in the near UV to 2000 nm in the IR.Vitreosil® opt..
Modulus of Elasticity 74.0 GPa
10700 ksi
Saint-Gobain Vitreosil® Clear Fused Quartz Tubing
Electrically fused quartz is recognized for its combination of purity, chemical inertness, physical stability, thermal shock resistance, high electrical resistivity, and high operating temperatures...
Modulus of Elasticity 74.0 GPa
10700 ksi
Saint-Gobain Puropsil® B Infrared Grade Low [OH] Optical Fused Quartz
Puropsil® B optical infrared fused quartz is manufactured from naturally occurring quartz crystal using a plasma process to ensure a low OH. It has excellent IR transmission with a useful IR tra..