Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 72.4 GPa | 10500 ksi | AA2024 |
Alcoa 2324-T39 Aluminum Plate Alloy 2324-T39 is a higher strength version of alloy 2024-T351 and is a purity controlled composition variant of alloy 2024. It was developed for tension-dominated, fatigue and fracture critical pl.. |
|||
Modulus of Elasticity | 72.4 GPa | 10500 ksi | |
Constellium Alumold® 350 Aluminum Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti.. |
|||
Modulus of Elasticity | 72.4 GPa | 10500 ksi | |
Potters Industries Spheriglass® 3000E Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |