Polymer Property : Modulus of Elasticity = 700 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D638
RTP Company RTP 1300 AR 5  Polyphenylene Sulfide (PPS) Aramid Fiber 5%  (discontinued **)<
Aramid Fiber 5%Comments:Aramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for..
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D638
RTP Company RTP 4000 AR 10 TFE 15  Polyphthalamide (PPA) Aramid Fiber 10% - PTFE 15%  (disco
Aramid Fiber 10% - PTFE 15%Comments:Aramid FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provi..
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D638
RTP Company RTP 2100 AR 15  Polyetherimide (PEI) Aramid Fiber 15%  (discontinued **)
Aramid Fiber 15%Comments:Aramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D638
RTP Company RTP 3102  Perfluoroalkoxy (PFA) Glass Fiber 15%  (discontinued **)
Glass Fiber 15%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Modulus of Elasticity 4.83 - 33.8 GPa
700 - 4900 ksi
Average value: 23.6 GPa Grade Count:21
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D638
RTP Company RTP 201D L  Nylon 6/12 (PA 6/12) Glass Fiber 10% - Lubricated  (discontinued **)
Glass Fiber 10% - LubricatedComments:Glass FiberLubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided b..
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D638
RTP Company RTP 202D TFE 10  Nylon 6/12 (PA 6/12) Glass Fiber 15% - PTFE 10%  (discontinued
Glass Fiber 15% - PTFE 10%Comments:Glass FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provide..
Modulus of Elasticity 4.83 - 5.52 GPa
700 - 800 ksi
ASTM D638
Lord Adhesives Fusor® 380NS / 383NS Epoxy Adhesive
LORD Fusor® 380NS/383NS adhesive is a two-part, rapid-cure epoxy adhesive used to bond fiberglass reinforced plastics (FRP), sheet molded compounds (SMC) and metals.All information provided by Lo..
Modulus of Elasticity 4.83 GPa
700 ksi
In Tension; ASTM D638
Devcon Magic Bond™ Epoxy Putty
Emergency Repair ProductsComments: Two-part epoxy putty stick seals leaks and repairs gouges in steel, aluminum, wood, fiberglass, concrete and ceramics. Cures rock-hard and can be painted, sanded,..
Modulus of Elasticity >= 4.83 GPa
>= 700 ksi
ASTM D638
Arlon AD260A PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs
For RF & Microwave Printed Circuit Boards. Low Loss PTFE and Ceramic Filled Composite Dielectric Constant (2.60)Low Dielectric Loss (Loss Tangent)Low Profile Copper (lower conductive losses)Low Z-d..
Modulus of Elasticity 4.83 GPa
700 ksi
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive
3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a pa..
Modulus of Elasticity >= 4.83 GPa
>= 700 ksi
ASTM D638
Arlon AD350A PTFE/Woven Fiberglass/Ceramic Filled Composite
Tighter Dielectric Tolerance Low Z-Axis Thermal ExpansionCeramic Filled PTFEHigh Thermal ConductivityLarge Panel SizeBenefits:Higher Consistency of PerformanceSuperior PTH AdhesionHeat Dissipation a..
Modulus of Elasticity 4.83 - 17.2 GPa
700 - 2500 ksi
Average value: 10.3 GPa Grade Count:28
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values..
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D638
RTP Company RTP 202C FR  Nylon 11 (PA 11) Glass Fiber 15% - Flame Retardant  (discontinued *
Glass Fiber 15% - Flame RetardantComments:Glass FiberFlame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information ..
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D638
RTP Company RTP 225D  Nylon 6/12 (PA 6/12) Mineral 20%  (discontinued **)
Mineral 20%Comments:MineralUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this pro..
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D638
RTP Company RTP 1400 AR 15  Polyethersulfone (PES) Aramid Fiber 15%  (discontinued **)
Aramid Fiber 15%Comments:Aramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D638
RTP Company RTP 1401 B L  Polyethersulfone (PES) Glass Fiber 10% - Lubricated  (discontinued
Glass Fiber 10% - LubricatedComments:Glass FiberLubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided b..
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D638
RTP Company RTP 1401 N L  Polyethersulfone (PES) Glass Fiber 10% - Lubricated - High Viscosity &n
Glass Fiber 10% - Lubricated - High ViscosityComments:Glass FiberHigh ViscosityLubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect pr..
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D638
RTP Company RTP 1402 N Z  Polyethersulfone (PES) Glass Fiber 15% - FDA Type - High Viscosity &nbs
Glass Fiber 15% - FDA Type - High ViscosityComments:Glass FiberFDA CompliantHigh ViscosityUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect p..
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D638
RTP Company RTP 3202  Ethylene Tetrafluoroethylene (ETFE) Glass Fiber 10%  (discontinued **)
Glass Fiber 10%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D638
RTP Company RTP 202B TFE 15  Nylon 6/10 (PA 6/10) Glass Fiber 15% - PTFE 15%  (discontinued
Glass Fiber 15% - PTFE 15%Comments:Glass FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provide..
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D412
RTP Company RTP 1205-70D TFE 20  Polyurethane Thermoplastic Elastomer (TPU) Glass Fiber 30% - PTFE 20% - 70 Shore D
Glass Fiber 30% - PTFE 20% - 70 Shore DComments:Glass FiberPTFE Lubricated70-D DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect pro..
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D638
RTP Company RTP 4000 AR 20  Polyphthalamide (PPA) Aramid Fiber 20%  (discontinued **)
Aramid Fiber 20%Comments:Aramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..