Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 67.0 GPa | 9720 ksi | |
Kaiser 6033 T6, T651 Rod & Bar Alloy 6033 is a higher strength version of alloy 6061, approaching properties typically obtainable with 2000 series alloys. The alloy was developed to also offer improved machinability over 6061. Th.. |
|||
Modulus of Elasticity | 67.0 GPa | 9720 ksi | |
Kaiser 6033 T8 Rod & Bar Alloy 6033 is a higher strength version of alloy 6061, approaching properties typically obtainable with 2000 series alloys. The alloy was developed to also offer improved machinability over 6061. Th.. |