Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 66.0 GPa
9570 ksi
Schott AF 45 Thin Borosilicate Glass
AF 45 is an alkali-free modified borosilicate glass with a high content of BaO and Al2O3. AF 45 with, its specific properties and large range of different thicknesses with tight tolerances, is exc..
Modulus of Elasticity 66.0 GPa
9570 ksi
Schott Glass 8487 Borosilicate Glass
Borosilicate glass for sealing to tungsten Backlights, flash lamps, lamp bulbs, exhaust and flare bulbs The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is ..
Modulus of Elasticity 66.0 GPa
9570 ksi
Schott Glass 8687 Borosilicate Glass
Borosilicate glass for sealing to tungsten, defined UV absorption, stabilized against solarization Backlights The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromi..
Modulus of Elasticity 66.0 GPa
9570 ksi
Schott KZFS12 Glass
Information Provided by SCHOTT North America, Inc.
Modulus of Elasticity 66.0 GPa
9570 ksi
Schott N-KF9 Glass
Information Provided by SCHOTT North America, Inc.
Modulus of Elasticity 66.0 GPa
9570 ksi
Schott N-KZFS2 Glass
Information Provided by SCHOTT North America, Inc.