Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 6.10 GPa | 885 ksi | |
Lehmann & Voss LUVOCOM® 1105-7777 PEEK, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Isotropic shrinkage characteristics.Emergency running property.Information provided by Leh.. |
|||
Modulus of Elasticity | 6.10 GPa | 885 ksi | ISO 527-1/-2 |
BASF Ultramid® FRee B3U31G4 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Modulus of Elasticity | 6.10 GPa | 885 ksi | Conditioned; ISO 178 |
Addiplast Addinyl C2 V40 Nylon 66/6, 40% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Modulus of Elasticity | 6.10 GPa | 885 ksi | ISO 527-1/-2 |
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass fiber reinforced injection molding grade e.g. for internal gas pressure applications such as flashing direction switch gears, automobile mirror housings and wheels of mountain.. |
|||
Modulus of Elasticity | 6.10 GPa | 885 ksi | Conditioned; ISO 178 |
Addiplast Addinyl C2 ZV40 Nylon 66/6, 40% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |