Polymer Property : Modulus of Elasticity = 56.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 56.0 GPa
8120 ksi
Schott Glass 8532 Soft Glass
Soft glass, free from Na, of high lead content, lower sealing temperature than glass 8531, high dielectric constant Encapsulation of semiconductor components at low temperature (diodes)Information ..
Modulus of Elasticity 56.0 GPa
8120 ksi
Schott SF1 Glass
Information Provided by SCHOTT North America, Inc.
Modulus of Elasticity 56.0 GPa
8120 ksi
Schott SF4 Glass
Information Provided by SCHOTT North America, Inc.
Modulus of Elasticity 56.0 GPa
8120 ksi
Schott SF5 Glass
Information Provided by SCHOTT North America, Inc.