Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 385 GPa | 55800 ksi | |
Plansee DENSIMET® D185 Tungsten-Nickel-Iron Alloy Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d.. |