Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 5.10 - 37.0 GPa @Temperature 60.0 - 150 °C |
740 - 5370 ksi @Temperature 140 - 302 °F |
Average value: 15.9 GPa Grade Count:8 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |