Modulus of Elasticity 35.2 GPa
5100 ksi
Effective Modulus
Hardwire 12x-12-12 Medium Density Composite
The 12X Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 12X wire cord is used where the traits of high tensile strain, excellent conformabi..