Polymer Property : Modulus of Elasticity = 5.70 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 5.70 GPa
827 ksi
ISO 527-2
Tisan TISLAMID® 66 15% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..