Mechanical Properties Metric English Comments
Modulus of Elasticity 1.68 - 5.40 GPa
244 - 783 ksi
Average value: 3.00 GPa Grade Count:22
Overview of materials for Epoxy, High Temperature
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val..
Modulus of Elasticity 0.950 - 5.40 GPa
138 - 783 ksi
Average value: 2.41 GPa Grade Count:147
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..