Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 5.25 GPa | 761 ksi | ISO 527-2 |
Tisan TISLAMID® 66 30% Mineral Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |