Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 33.0 GPa | 4790 ksi | |
Lehmann & Voss LUVOCOM® 1105-7751 PEEK, with carbon fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Modulus of Elasticity | 33.0 GPa | 4790 ksi | |
Lehmann & Voss LUVOCOM® 1301/XCF/30 N PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Modulus of Elasticity | 33.0 GPa | 4790 ksi | in <100> direction |
Mateck Potassium Bromide (KBr) Optical crystals |