Polymer Property : Modulus of Elasticity = 466 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 3.21 GPa
466 ksi
50 mm/min; ASTM D638
LG Chemical 92HR SAN Resin
Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include automobile battery cases, water meter case..