Mechanical Properties Metric English Comments
Modulus of Elasticity 0.317 GPa
46.0 ksi
ASTM D638M
DSM Somos® 8110 Epoxy Photopolymer  (discontinued **)
DescriptionDSM Somos® 8110 is a high-speed liquid photopolymer that produces flexible, high-impact-strength, accurate parts using stereolithography machines. It has a wide processing latitude and ..
Modulus of Elasticity 0.317 GPa
46.0 ksi
Secant; ASTM D638
Huntsman PE1201 EVA Film Extrusion  (discontinued **)
2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Good optical, medium impact strength, and good processability.Applications: Film extrusion: heavy duty packaging.FDA Notes: Conforms to FDA ..