Polymer Property : Modulus of Elasticity = 454 ksi
Polymer Property :
Modulus of Elasticity =
454 ksi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Modulus of Elasticity
3.13
GPa
454
ksi
GB/T 1040
Beijing Evergrow Resources Oilon
Information provided by Beijing Evergrow Resources.