Polymer Property : Modulus of Elasticity = 45000 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 290 - 310 GPa
42100 - 45000 ksi
Youngs Modulus
MMCC Al/Al2O3 Continuous Fiber Aluminum Matrix Composite
Cast, reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).