Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 301 GPa | >= 43700 ksi | Minimum |
Materion E20 Beryllium/BeO Composite, 20 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |