Mechanical Properties Metric English Comments
Modulus of Elasticity 15.0 - 42.0 GPa

@Temperature 60.0 - 150 °C
2180 - 6090 ksi

@Temperature 140 - 302 °F
Average value: 29.5 GPa Grade Count:1
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Modulus of Elasticity 0.0370 - 42.0 GPa
5.37 - 6090 ksi
Average value: 7.22 GPa Grade Count:739
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..