Polymer Property : Modulus of Elasticity = 4.314 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.02974 GPa
4.314 ksi
ASTM D412 Method A
Seals Eastern 7204 Ethylene-Propylene Rubber
Y267-Type EPDM for geothermal steam service. Ultra-Low compression set.Information provided by Seals Eastern, Inc.