Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.41 - 4.14 GPa | 350 - 600 ksi | Average value: 3.58 GPa Grade Count:17 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Modulus of Elasticity | 3.10 - 4.14 GPa | 450 - 600 ksi | Average value: 3.54 GPa Grade Count:11 |
Overview of materials for Nylon 612, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Modulus of Elasticity | 2.76 - 4.14 GPa | 400 - 600 ksi | Average value: 3.22 GPa Grade Count:6 |
Overview of materials for Nylon 11 with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ.. |