Polymer Property : Modulus of Elasticity = 4.06 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0280 GPa
4.06 ksi
ASTM D412
KKPC KOSYN KTR 401 Thermoplastic Elastomer (TPE)
Thermoplastic Elastomer (TPE)Characteristics: KOSYN KTR101 is linear block copolymer made by solution polymerization which polymerizes butadiene and styrene in organic solvent. It is thermoplastics ..