Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.75 - 15.2 GPa | 399 - 2200 ksi | Average value: 8.65 GPa Grade Count:31 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |