Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.59 - 12.27 GPa @Temperature -40.0 - 120 °C |
376 - 1780 ksi @Temperature -40.0 - 248 °F |
Average value: 6.33 GPa Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |