Polymer Property : Modulus of Elasticity = 35200 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 243 GPa
35200 ksi
Kennametal Stellite Stellite® 33
Completely non-magnetic. Specific Electrical Resistance: 39.8 µOhm/in^3.Applications: standard tool bits, tipped tools, form tools, milling cutter blades, wood working tools, reamer blades, cut-o..