Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.37 - 2.65 GPa | 344 - 384 ksi | UV Postcure; ASTM D368M |
DSM Somos® GP Plus 14122 Somos® GP Plus 14122 is a low-viscosity stereolithography resin with an opaque white appearance. This material mirrors production plastics like ABS and PBT, making it an ideal choice for virtually .. |
|||
Modulus of Elasticity | 2.37 GPa | 344 ksi | |
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |