Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.235 GPa | 34.1 ksi | Secant; ASTM D638 |
Huntsman PE1403 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA Copolymer, DMF listed and FDA compliantFeatures: High clarity film with good toughness and flexibility at low temperatures.Applications: Film extrusion: frozen food and general .. |
|||
Modulus of Elasticity | 0.235 GPa | 34.1 ksi | Secant; ASTM D638 |
Huntsman PE1451 EVA Film Extrusion
(discontinued **) 4.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |