Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.83 - 2.21 GPa | 265 - 320 ksi | Average value: 2.07 GPa Grade Count:12 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max.. |